CrystaLac Amber Toned Sanding Sealer can be applied by either brushing or spraying. Its thin viscosity makes it easy to spread and allows it to penetrate into porous woods. Sand bare wood with 220 grit sandpaper. Apply 1 coat of Sanding Sealer and allow to dry. Lightly scuff sand to remove any raised grain fibers. Apply an additional 1 to 2 coats to seal wood and provide an excellent surface that will be ready to topcoat.
CrystaLac Sanding Sealer can also be used as a pre-stain conditioner. Apply 1 coat of Sanding Sealer to bare wood and allow to dry. Sand back down to bare wood leaving the sealer only in the wood grain and pores. Apply stain and allow it to thoroughly dry. Oil based stains can take up to a week to dry. Apply another 1 to 2 coats of Sanding Sealer over the dried stain. This will help to seal the stain color down and keep it from spreading. It is now ready for a clear top coat.
Dry Time: 30 min to 1 hour
Recoat Time: 1 to 2 hours
Coverage: 400 to 500 sq. ft. per Gallon
Do Not use tack cloths or stearated sandpaper. Do Not Freeze.
Warranty: Test to your satisfaction on scrap material before using. The manufacturer, The CrystaLac Company, will only replace defective product. Under no circumstances will the manufacturer or distributors be responsible for the cost of application labor, refinishing expenses, or any costs in excess of the purchase price of the container.
Caution: Keep out of reach of children! Do not ingest. Avoid contact with skin and eyes. Do not breathe vapors. Use with adequate ventilation. When spraying or sanding, use an OSHA approved mask. V.O.C. is less than 1.4 Lbs. per gallon.
Disposal: Consult your local sanitation department. Do not dump on the ground.
- Penetrates and Prepares wood for Top Coats
- Enhances and Warms Wood Tone
- Seals wood fibers and minimizes grain raise
CrystaLac Amber Toned Sanding Sealer can be applied by either brushing or spraying. Its thin viscosity makes it easy to spread and allows it to penetrate into porous woods. Sand bare wood with 220 grit sandpaper. Apply 1 coat of Sanding Sealer and allow to dry. Lightly scuff sand to remove any raised grain fibers. Apply an additional 1 to 2 coats to seal wood and provide an excellent surface that will be ready to topcoat.
CrystaLac Sanding Sealer can also be used as a pre-stain conditioner. Apply 1 coat of Sanding Sealer to bare wood and allow to dry. Sand back down to bare wood leaving the sealer only in the wood grain and pores. Apply stain and allow it to thoroughly dry. Oil based stains can take up to a week to dry. Apply another 1 to 2 coats of Sanding Sealer over the dried stain. This will help to seal the stain color down and keep it from spreading. It is now ready for a clear top coat.
Dry Time: 30 min to 1 hour
Recoat Time: 1 to 2 hours
Coverage: 400 to 500 sq. ft. per Gallon
Do Not use tack cloths or stearated sandpaper. Do Not Freeze.
Warranty: Test to your satisfaction on scrap material before using. The manufacturer, The CrystaLac Company, will only replace defective product. Under no circumstances will the manufacturer or distributors be responsible for the cost of application labor, refinishing expenses, or any costs in excess of the purchase price of the container.
Caution: Keep out of reach of children! Do not ingest. Avoid contact with skin and eyes. Do not breathe vapors. Use with adequate ventilation. When spraying or sanding, use an OSHA approved mask. V.O.C. is less than 1.4 Lbs. per gallon.
Disposal: Consult your local sanitation department. Do not dump on the ground.